R20P无汞锌锰电池正极配方和工艺  

Positive formula and technology of R20P mercury-free Zn/MnO_2 battery

在线阅读下载全文

作  者:吴立柔 

机构地区:[1]宁波市力达电池有限公司,浙江宁波315051

出  处:《电池工业》2001年第5期217-219,共3页Chinese Battery Industry

摘  要:正确选择电池正极配方和工艺是氯化锌型电池制造技术的关键之一。扼要总结了R20P无汞锌锰电池正极配比中的电液的氯化锌浓度、电液中氯化铵的掺加量、水份的含量、乙炔黑比例、电解锰比例等5项因素,按5个位级进行正交试验,按5个因素对3.9Ω连放和间放影响程度的大小进行主次排列,并进行原因分析,确定了正极配方的最佳范围,指出了正极制造过程中拌粉、打芯、复压各个工序的注意点。It is importantfor the productionof zinc chloride battery that we must choose correctly the positive formula and technics.The concentration of ZnCl 2 and NH 4 Cl,water content,ethyne carbon black content,EMDcontent in the battery positive formula were summerizedconcisely.Andcomplywith the five above mentionedfactors,an orthogonal test was carried out.Accordingto the effects on3.9Ω discharge(continuousand discontinuous),the five factors were arrangedfrom staple to subordination.Andthe reason was analyze...

关 键 词:无汞锌锰电池 正极配方 拌粉 打芯 复压 

分 类 号:TM911.14[电气工程—电力电子与电力传动]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象