Impermeability of Tunnel Structural material after Exposure to High Temperature  

Impermeability of Tunnel Structural material after Exposure to High Temperature

在线阅读下载全文

作  者:张风臣 

机构地区:[1]Key Laboratory for Silicate Materials Science and Engineering (Ministry of Education) Wuhan University of Technology, Wuhan 430070, China

出  处:《Journal of Wuhan University of Technology(Materials Science)》2006年第z1期162-166,共5页武汉理工大学学报(材料科学英文版)

基  金:Funded by National High-Tech Research and Development Program of China(No.2005AA332010)

摘  要:Impermeability of tunnel structural material after exposure to high temperature determines residual service life and security. The present study explores impermeability deterioration and water absorption change (expressed as w(T, t)) of tunnel structural material after exposure to 200℃, 300℃, 400℃, 500℃, and 600℃respectively. Structural cementitious material was devised according to the requirements of segment used in Yangtze River tunnel of Wuhan which has been in constructing. Effect of high temperature on impermeability is evaluated by impermeability deterioration factor (abbr. IDF) and w(T, t).Testing results indicate that impermeability of concrete decreases with the increase of temperature up to 600℃, and serious impermeability deterioration occurs at temperature above 300℃. Furthermore, concrete with higher impermeability is more sensitive to high temperature above 400℃.Impermeability of tunnel structural material after exposure to high temperature determines residual service life and security. The present study explores impermeability deterioration and water absorption change (expressed as w(T, t)) of tunnel structural material after exposure to 200℃, 300℃, 400℃, 500℃, and 600℃respectively. Structural cementitious material was devised according to the requirements of segment used in Yangtze River tunnel of Wuhan which has been in constructing. Effect of high temperature on impermeability is evaluated by impermeability deterioration factor (abbr. IDF) and w(T, t).Testing results indicate that impermeability of concrete decreases with the increase of temperature up to 600℃, and serious impermeability deterioration occurs at temperature above 300℃. Furthermore, concrete with higher impermeability is more sensitive to high temperature above 400℃.

关 键 词:high temperature IMPERMEABILITY IDF w(T  t) 

分 类 号:U454[建筑科学—桥梁与隧道工程]

 