攀成钢150方坯生产低碳低硅钢冶炼连铸工艺试验  

LOW-CARBON AND LOW-SILICON STEEL SMELTING AND CONTINUOUS CASTING PROCESS OF 150 SQUARE BILLET PRODUCTION OF PANGANG GROUP CHENGDU IRoN & STEEL CO. LTD.

在线阅读下载全文

作  者:易兴俊[1] 万朝明[1] 李荣芳[1] 张珉[1] 

机构地区:[1]攀钢集团成都钢铁有限责任公司,四川成都610066

出  处:《四川冶金》2008年第4期25-28,共4页Sichuan Metallurgy

摘  要:介绍了攀成钢采用铁水→80 t转炉→LF钢包精炼炉→五机五流方坯连铸工艺生产低碳低硅BL2钢的工艺试验。通过控制转炉终点碳、出钢下渣,制定合理脱氧工艺、LF炉Ca处理工艺,强化连铸保护浇铸等技术措施,解决了生产低碳低硅钢存在的脱氧、浇铸、成份控制等技术难题,为公司大量开发此钢种奠定了技术基础。This article describes the study on the low-carbon and low-silicon BL2 steel production process of PGGCSST as liquid iron→80 t converter→LF refined-smelting ladle furnace→5-strand square billet casting.By controlling end-point carbon and tapping and slag amount,using reasonable deoxidizing method and Ca processing method in LF furnace,and strengthening protective pouring,the process has solved the technical problems of low-carbon and low-silicon steel production such as deoxidation,pouring and element contr...

关 键 词:低碳低硅钢 冶炼连铸工艺 脱氧 浇铸 成份控制 

分 类 号:TF777[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象