混凝土早期收缩性能试验研究  被引量:11

Experimental research on early age shrinkage of concrete by eddy current method

在线阅读下载全文

作  者:杨文武[1,2] 钱觉时[1] 范英儒[1] 

机构地区:[1]重庆大学材料科学与工程学院,重庆400045 [2]大连民族学院土木建筑工程学院,大连116600

出  处:《深圳大学学报(理工版)》2009年第1期81-85,共5页Journal of Shenzhen University(Science and Engineering)

基  金:国家自然科学基金资助项目(50572127)

摘  要:运用电涡流方法测量混凝土早期收缩,研究了水胶比、引气剂和矿物掺合料等因素对混凝土早期收缩性能的影响.结果表明,水胶比为0.45的混凝土3d收缩率可达到78×10-6,复掺硅灰矿渣和引气剂时,混凝土3d收缩率达到113×10-6;随引气剂掺量增大,混凝土早期收缩增加,但在正常掺量范围内引气剂的影响较小;混凝土成型后400~1500min为水泥水化放热高峰,其早期收缩曲线出现膨胀或收缩减缓现象.To understand early age shrinkage of concrete in order to get high performance concrete,an eddy current method was used to measure the early age shrinkage of concrete with different water-binder ratios and mineral admixtures such as fly ash,slag and silica fume and air-entraining admixture.The results show that the shrinkage of concrete with water-binder ratio of 0.45 reached 78×10-6 and that of concrete incorporating slag,silica fume and air-entraining admixture reached 113×10-6 in 3 days.Addition of air-e...

关 键 词:混凝土 收缩 电涡流 早期 引气剂 

分 类 号:TU528.01[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象