新型高温永磁体的研制  被引量:1

Research and manufacture of a new type of high temperature permanent magnets

在线阅读下载全文

作  者:彭元东[1] 李丽娅[1] 杜娟[1] 周庭[1] 陈忠文[1] 易健宏[1] 

机构地区:[1]中南大学粉末冶金国家重点实验室,湖南长沙410083

出  处:《粉末冶金材料科学与工程》2003年第3期237-241,共5页Materials Science and Engineering of Powder Metallurgy

摘  要:通过分析影响磁体高温性能的因素,设计了新磁体的成分为:Cu含量高,Fe含量低,Zr适量,Sm含量高;采用粉末冶金工艺制备了高温Sm_2(CoFeCuZr)_(17)永磁体。制得的磁体室温磁性能为:B_r1.075 T,H_(ei)2 098.2 kA/m,H_(eb) 776.1 kA/m,H_k843.8 kA/m,(BH)_(max)210.0 kj/m^3;在200℃时的磁性能为:B_r0.991 T,H_(ci)1 175.7 kA/m,H_(cb)531.7 kA/m,H_k577.9 kA/m,(BH)_(max)172.5 kJ/m^3;矫顽力温度系数β(20~200℃)为-0.24%/℃。经理论分析和实验验证,磁体的使用温度均超过400℃,为高温环境(高于400℃)提供了一种实用性永磁材料。By the analysis of high temperature magnetic properties of magnets, the component of alloy is designed at the principle of high Cu, reduced Fe, fitted Zr and high Sm. Then the Sm_2 (CoCuFeZr)_(17) permanent magnets are manufactured with the technology of powder metallurgy. The room magnetic properties of magnets have B_r 1.075 T, H_(ci) 2098.2 kA/m, H_(cb) 776.1 kA/m, H_k 843.8 kA/m and (BH)_(max) 210.0 kJ/m^3. The 200 ℃ magnetic properties of magnets have B_r 0.991 T, H_(ci) 1175.7 kA/m, H_(cb) 531.7 kA/m, H_k 577.9 kAm and (BH)_(max) 172.5 kJ/m^3. The temperature coefficient of coercivity β(20-200℃) is -0.24%/℃. The theory analysis and experiment result show that the maximum operated temperature of magnets exceed 400 ℃. It provides a kind of practical high temperature magnets.

关 键 词:高温磁体 2:17型SmCo合金 成分设计 制造工艺 磁性能 

分 类 号:TM273[一般工业技术—材料科学与工程] TG132.2[电气工程—电工理论与新技术]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象