微波法合成纳米TiO_2及Fe^(3+)掺杂纳米TiO_2粉体的研究  被引量:4

Hydrothermal synthesis and characterization of TiO_2 nanometer powder doped with Fe^(3+) in terms of microwave

在线阅读下载全文

作  者:周晓明[1] 张培新[1] 刘剑洪[1] 李静[1] 陈玉辉[1] 

机构地区:[1]深圳大学师范学院化生系,深圳518060

出  处:《化工新型材料》2004年第7期16-19,共4页New Chemical Materials

基  金:深圳市科技计划项目 (编号 :2 0 0 2 1 9)

摘  要:通过控制盐的水解和微波辐射制备出晶粒尺寸为 6~ 2 5nm的TiO2 、Fe/TiO2 粉体。对水解温度、陈化时间、微波辐射的影响进行研究 ,发现TiO2 水解温度在 70~ 80℃、Fe/TiO2 水解温度在 6 5℃时 ,晶粒尺寸较小 ,而室温陈化时间的长短对晶粒尺寸没有大的影响 ,样品未微波辐射与微波辐射的晶粒尺寸、热性质等存在明显不同。通过XRD、TG DSC。The powders of TiO 2, Fe/TiO 2, which crystallite sizes were 6~25nm were prepared by the methods of controlling salt hydrolysis and microwave radiation. After researching into the effect of hydrolytic temperature , ageing time and microwave , we found that the crystallite sizes of TiO 2 and Fe/TiO 2 were small when the hydrolytic temperature is centigrade from 60 to 80,but the ageing time within indoors temperature has not much effect on the crystallite size. There are obviously differences between non-microwave and microwave to nano-TiO 2 in crystallite sizes , thermal characters and so on. Obtained nanometer powders were measured by XRD, TG-DSC and TEM.

关 键 词:微波水热法 合成 纳米TIO2粉体 氧化铊 Fe3^+掺杂 陈化时间 水解温度 

分 类 号:O614[理学—无机化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象