Low-cost oriented preparation of ultra fine xonotlite fibers  

Low-cost oriented preparation of ultra fine xonotlite fibers

在线阅读下载全文

作  者:NI Wen, CHEN Shuxiang, and ZHU Lin 

出  处:《Rare Metals》2004年第3期230-230,共1页稀有金属(英文版)

摘  要:Nanometer-sized xonotlite fibers have great potential application in many fields. The traditional method of preparing ultra fine xonotlite fibers uses the ultra fine and highly active silica as the major raw materials, which is not only expensive but also difficult to prepare the xonoflite fibers with diameters around 100 nm. In this study, the ultra fine xonotlite fibers with diameters around 100 nm were prepared by an autoclaving method. The preparation was low-cost oriented by using natural powder quartz and lime as the major raw materials. The intergrowth of the fibers formed thin shell hollow balls or ellipsoids, namely the secondary particles. The length of the nanometer-sized xonotlite fibers was around several microns. The fibers and their secondary particles were produced at 216℃ for 6 h with a continuous stirring of 300-500 r/min. Zirconium oxychloride was used as an additive. The experiments show that zirconium oxychloride has an enormous effect on the growing habit of xonotlite crystals and plays an important role in controlling the diameter of xonotlite fibers.Nanometer-sized xonotlite fibers have great potential application in many fields. The traditional method of preparing ultra fine xonotlite fibers uses the ultra fine and highly active silica as the major raw materials, which is not only expensive but also difficult to prepare the xonoflite fibers with diameters around 100 nm. In this study, the ultra fine xonotlite fibers with diameters around 100 nm were prepared by an autoclaving method. The preparation was low-cost oriented by using natural powder quartz and lime as the major raw materials. The intergrowth of the fibers formed thin shell hollow balls or ellipsoids, namely the secondary particles. The length of the nanometer-sized xonotlite fibers was around several microns. The fibers and their secondary particles were produced at 216℃ for 6 h with a continuous stirring of 300-500 r/min. Zirconium oxychloride was used as an additive. The experiments show that zirconium oxychloride has an enormous effect on the growing habit of xonotlite crystals and plays an important role in controlling the diameter of xonotlite fibers.

关 键 词:LOW-COST ultra fine fibers XONOTLITE ADDITIVE 

分 类 号:O613[理学—无机化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象