TCS法生产多孔细旦涤纶长丝工艺的研究  被引量:1

Production of porous fine denier PET filament with TCS

在线阅读下载全文

作  者:王延伟[1] 孟春丽[1] 

机构地区:[1]河南纺织高等专科学校,郑州450007

出  处:《聚酯工业》2004年第6期47-49,共3页Polyester Industry

摘  要:探讨了用TCS法生产90dtex/108f涤纶长丝时,切片含水率、纺丝温度、纺丝速度、热管位置、热管温度等工艺参数的选择.结果表明:干切片中水的质量分数小于18×10-6,热管至喷丝板距离920~960mm、热管温度176~183℃,卷绕速度为4.2~4.4km/min时,可生产出优质涤纶长丝。During the production of the 90 dtex/108 f porous fine denier polyester filaments with TCS,we should attach the importance to the process parameters ,such as moisture content of chips ,spinning temperature and speed,thermo-channel temperature and postion. The results showed that the good porous fine denier polyester filaments could be produced when moisture content of dried chips is less than 18 μg/g,the distance between the thermo-channel and spinneret is 920~960 mm, the thermo-channel temperature is 176~183 ℃,and the take-up speed is 4.2~4.4 km/min.

关 键 词:涤纶长丝 多孔细旦 热管纺丝 

分 类 号:TQ342.21[化学工程—化纤工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象