平武石坎锰精矿冷固球团还原焙烧试验研究  

STUDIES OF REDUCING ROAST OF PING WU MANGANESE CONCENTRATE PELLETS OF COLD HARDENING

在线阅读下载全文

作  者:李华成[1] 

机构地区:[1]长沙矿冶研究院

出  处:《中国锰业》1994年第6期33-37,共5页China Manganese Industry

摘  要:本研究采用冷固球团+回转窑还原焙烧工艺来处理平武锰精矿,球团内配碳含碳量为4.4%,粒度3~5mm,还原温度为900℃,时间为1h,还原过程中不需外配还原剂。经过6h的0.6m×3m回转窑还原焙烧连续试验取得了MnO_2最高还原率达93.96%,平均还原率为91.85%,产能为2.4t/m ̄3d的好结果。这些结果为工业试验及生产提供了可靠的技术依据。Reducing roast is used to deal with Ping Wu manganese concentrates inthe form of cold hardening pellets which contain 4.4%carbon and have particle sizes of 3mmto 5mm. No extra reducing agent is needed under the conditions of 900℃ temperature and 1hour time for the reduction.Results of continuous test for the reducing roast in a 0.6m by3m rotary furnace for 6 hours show that the maximum and average percentage of reducedMnO_2 are 93. 96%and 91.5%respectively and the throughput capacity is 2.4t/m ̄3·d.Theresults can be used for the basis of the corresponding trial and production.

关 键 词:锰精矿 回转窑 还原焙烧 

分 类 号:TF521.6[冶金工程—钢铁冶金] TF111.13

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象