含碳铬矿球团的造球及直接还原  被引量:1

Balling and Direct Reducing Experiments of Carbon-Bearing Chromite Powder

在线阅读下载全文

作  者:徐荣军[1] 倪瑞明[1] 张圣弼[1] 马中庭[1] 

机构地区:[1]北京科技大学物理化学系

出  处:《北京科技大学学报》1995年第4期383-386,共4页Journal of University of Science and Technology Beijing

摘  要:研究了原料粒度、粘结剂的用量、配碳量等因素对铬铁矿球团生球性能的影响,以及温度和还原时间对金属化率的影响。结果表明1350℃还原15min,铬金属化率达90%以上配碳量应比理论配碳量过量20%。用1:3的H2S04对还原球团采用加热回流法溶样,解决了金属铬及金属铁的化学分析方法。Balling and reducing experiments of carbon-bearing chromite powder were carried out in laboratory. The effect of grain size of raw materials, amount of binder and carbon and other factors on the green pellet properties and the influence of reducing temperature and time on the metallization rate of carbon bearing chromite pellet were investigated. The results shown that the metallization rate of carbon-bearing chromite pellet of up to 90% under the reducing temperature of 1350℃, reducing time of 15 minutes, the amount of carbon exceed the the theoretical carbon requirement by 20%. By using heating reflux method and 1:3 H_2SO_4, the chemical analysing of metallic Cr and Fe becomes easier.

关 键 词:铬铁矿 直接还原 金属化球团 铁合金 铬铁 

分 类 号:TG641[金属学及工艺—金属切削加工及机床]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象