掺碳制备锂离子电池正极材料LiFePO_4  被引量:4

Preparation on cathode materials of LiFePO_4 doping carbon for lithium-ion battery

在线阅读下载全文

作  者:曲涛[1] 田彦文[1] 钟参云[1] 丁扬[1] 翟玉春[1] 

机构地区:[1]东北大学材料与冶金学院,辽宁沈阳110004

出  处:《分子科学学报》2005年第4期37-41,共5页Journal of Molecular Science

基  金:辽宁省自然科学基金资助项目(9810300702)

摘  要:采用固相法合成LiFePO4和掺碳的LiFePO4,并对不同掺碳量的 LiFePO4进行电化学性能测试,室温条件下,在0.1 C倍率下充放电,样品d (ωc=8.5%)的初始放电容量为151.7 mA·h/g.10次循环后,其放电比容量仍 有149.5 mA·h/g,容量损失较小.这表明,在合适的制备工艺条件下,掺碳能获 得结构稳定、电化学性能良好的锂离子电池正极材料LiFePO4.LiFePO4 and LiFePO4 doping carbon were prepared by solid-state reaction.Sample d(ωC=8.5%)had good electrochemical performance whose initial capacity was 151.7 mA·h/g. It retained specific capacity 149.5 mA·h/g after 10 circles and had small capacity fading at room temperature. It showed that LiFePO4 with steady structure and good electrochemical performance could be obtained in appropriate conditions.

关 键 词:锂离子电池 正极材料 LIFEPO4 掺碳 固相法 

分 类 号:O646[理学—物理化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象