免烧结免蒸养粉煤灰砖的力学性能及水化机理  被引量:1

Mechanical Property and Hydrating Mechanism of Non-sintering or Non-autoclave Fly Ash Brick

在线阅读下载全文

作  者:张海涛[1] 杨久俊[1] 张磊[1] 黄明[1] 马建丽[2] 

机构地区:[1]郑州大学材料工程学院,450052 [2]天津城市建设学院,3000384

出  处:《粉煤灰综合利用》2005年第6期25-27,共3页Fly Ash Comprehensive Utilization

基  金:国家自然科学基金(50472030);河南省重点科技攻关计划(423033000);天津市社会发展项目"粉煤灰微珠分离提取与深加工技术研究"资助

摘  要:以提取微珠后的粉煤灰残灰为主要原料(掺量为85%),辅以少量的钙质材料及微量的激发剂,通过研究不同原料配方、成型压力、养护方式对粉煤灰砖力学性能的影响,探索免烧结免蒸养承重粉煤灰砖的最佳制作工艺,通过粉煤灰砖的不同龄期的强度及微观结构,分析了粉煤灰残灰的激活及水化机理。This paper is about the best manufacturing process of Non-sintering or non-autoclave bearing fly ash brick. The residual fly ash (after extracting mierospheres) was used as the major material(mixture is 85%), mixed with little calcareous materials and minim excitant. The effect of different mixture ratios, forming pressure and earing modes on the mechanical property of brick was studied. The excitation and hydrating mechanism of residual fly ash were analyzed through the strength and mierostrueture of fly ash brick at different ages.

关 键 词:粉煤灰残灰  免烧结免蒸养 水化机理 

分 类 号:TU528.2[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象