SiC晶须增韧WC陶瓷刀具材料的研究  被引量:6

Study of WC Ceramic Tool Material by SiC Whisker Toughening

在线阅读下载全文

作  者:曹玉军[1] 刘杰[2] 

机构地区:[1]湘南学院,湖南郴州423000 [2]郴州职业技术学院,湖南郴州423000

出  处:《稀有金属与硬质合金》2005年第4期13-16,27,共5页Rare Metals and Cemented Carbides

摘  要:通过正交试验法对WC/SiCW陶瓷复合材料进行了成分和热压工艺参数优化,经优化制备的该类复合材料与纯WC材料相比,抗弯强度提高了约50%,断裂韧性提高了30%~40%,维氏硬度提高了10%~15%.切削试验数据证明,本试验制得的WC/SiCW复合陶瓷刀具材料的车削性能优于同类型硬质合金材料,表明通过SiCW替代金属粘结相来增韧补强WC陶瓷刀具材料的方法是可行的.The composition and hot-pressing parameters of WC/SiCw ceramic composite were optimized through orthogonal experiment. Compared with those of the pure WC, the bending strengh, fracture toughness and Vicker's hardness of the optimized WC/SiCw composite are increased by 50%, 30% -40%, and 10% - 15 % respectively. The cutting test results show that the optimized WC/SiCw composite ceramic cutting tool material exhibit superior turning properties to similar hard alloy material, indicating that it is feasible to toughen the WC ceramic cutting tool material by using SiCw instead of metallic binding phase.

关 键 词:复合陶瓷 晶须 热压 增韧强化 WC/SiCw 

分 类 号:TG148[一般工业技术—材料科学与工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象