Sm^(3+)掺杂CaO-SiO_2-B_2O_3发光玻璃的制备、表征及性质  被引量:4

Preparation and Fluorescence of Sm^(3+) Doped CaO-SiO_2-B_2O_3 Glasses

在线阅读下载全文

作  者:于健[1] 刘又年[1] 陈立妙[1] 黄可龙[1] 

机构地区:[1]中南大学化学化工学院,长沙410083

出  处:《无机化学学报》2006年第2期248-252,共5页Chinese Journal of Inorganic Chemistry

基  金:中南大学博士后基金资助项目

摘  要:用高温固相法合制备了以CaO-SiO2-B2O3为基质,Sm3+为激活离子的发光玻璃。对Sm3+的淬灭浓度、基质中的硼硅比例、其他稀土离子的敏化作用以及基质组成等因素对玻璃发光特性的影响进行了探讨,并用红外和X-衍射分析对样品的结构进行了表征。结果表明:当Sm3+掺杂的物质的量分数为1.2%,激发波长λ=404nm时,玻璃体60CaO-20SiO2-20B2O3∶1.2Sm3+的发光强度为4838A.U.(λ=606nm);这种发光玻璃具有将紫外及近紫外光转换为橙红色光的特点。少量的Eu3+的掺入,对玻璃体的发光起敏化作用;玻璃体中的组分CaO可被ZnO替代。Sm^3+ doped CaO-SiO2-B2O3 glasses were prepared with high temperature solid-state method. The effects of concentrations of doped Sm^3+, compositions and components of glass matrix, sensitive ions on fluorescence of glasses, were investigated. The structure of the glass was characterized by XRD and FFIR. The results show that the glasses can convert UV or near UV to orange. The fluorescence intensity of glass is 4838 A.U.(at =606 nm) with 404 nm excitation when the molar concentration of Sm^3+ is 1.2%. Eu^3+ can be used as sensitive ion to Sm^3+ doped CaO-SiO2-B203 glasses. ZnO can replace for CaO in glass matrix.

关 键 词:发光玻璃 SM^3+ 掺杂 制备 发光特性 

分 类 号:O613.72[理学—无机化学] O482.31[理学—化学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象