优质高碳钢高拉碳前期脱磷过程控制  被引量:25

Process control of dephosphorization in initial smelting period of combined blowing BOF for clean steel

在线阅读下载全文

作  者:刘跃[1] 刘浏[1] 佟溥翘[1] 赵继宇[2] 吴建鹏[2] 李小明[2] 王国平[2] 

机构地区:[1]钢铁研究总院工艺所,北京100081 [2]武汉钢铁(集团)公司,湖北武汉430083

出  处:《炼钢》2006年第2期27-29,共3页Steelmaking

摘  要:在分析了复吹转炉脱磷的热力学与动力学条件的基础上,利用复吹转炉吹炼前期(0~8min)低温的有利条件实现钢-渣充分脱磷、倒掉脱磷渣后进行少渣冶炼、高碳下出钢。以实现复吹转炉吹炼前期高效脱磷,吹炼前期的脱磷率达到75%-93%。The thermodynamics and kinetics of combined blown BOF dephosphorization is discussed, on the basic of which the fully dephosphorization in reaction of steel and slag, little slag smelting technology after getting rid of dephosphorizing slag , equating decarburization rate and tapping in the condition of high carbon is realized by the condition of smelting prior period (0-8min). Through above technology, the highly active dephosphorization of smelting prior period in BOF And dephosphorization ratio is obtained from 75 ting.

关 键 词:洁净钢 复吹转炉 冶炼前期 脱磷 

分 类 号:TF762[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象