锡槽中玻璃带收放量的计算  

The Calculating Formula for Shrinkage Allowance of Glass Ribbon Width in Tinbath

在线阅读下载全文

作  者:崔书庆 吴知方[2] 

机构地区:[1]洛阳玻璃集团玻璃股份有限公司,河南洛阳471009 [2]同济大学材料科学与工程学院,上海200092

出  处:《玻璃与搪瓷》2006年第2期34-37,共4页Glass & Enamel

摘  要:分析表明,生产同一厚度玻璃,在成形条件相同时,表面张力与玻璃纵向拉引产生的横向收缩对末对拉边机后玻璃带收缩率的影响不大。以5mm玻板为模式,导出锡槽中拉边机之杆放(收)量和拉边机后收缩率的计算公式。实验表明,计算值与实际值吻合较好,能较好指导生产。The analysis shows that when same thick glass sheet is produced in same forming conditions, the transverse shrinkage stress caused by surface tension and longitudinal dragging has little effects on shrinkage of glass ribbon behind the last pair of top rollers. Taking the 5ram thick sheet glass as example, a formula for calculating the shrinkage allowance of bar of top rollers has been deduced. It has been verified in practice that the calculating values are weU fitted to actual values. This means that the formula can be used for guiding real production.

关 键 词:浮法玻璃 拉边机 收放量 

分 类 号:TQ171.634[化学工程—玻璃工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象