用浮选工艺回收低品位细脉型黑白钨矿的试验研究  被引量:6

Recovery of Wolfram from Low-grade Ore in Stringer Vein

在线阅读下载全文

作  者:管则皋[1] 张先华[1] 梁冬云[1] 陈子起 

机构地区:[1]广州有色金属研究院,广东广州510651 [2]厦门钨业有限公司,福建厦门361000

出  处:《矿产综合利用》2006年第2期3-8,共6页Multipurpose Utilization of Mineral Resources

摘  要:采用浮选对低品位细脉型黑白钨矿石进行了选矿试验研究,试验结果表明:在原矿含WO30.23%、Mo0.018%、Cu0.013%的情况下,得到钨精矿品位63.31%、钨回收率86.64%,硫化矿含钼品位2.59%、钼回收率66.19%,含铜品位1.51%、铜回收率53.43%的技术指标,达到了有效回收钨和综合回收钼、铜的目的。A flotation process for recovery of wolfram mineral from a low-grade tungsten ore in stringer vein was described in this article. Flotation results indicated that the crude ore contains WO30.23%, Mo0. 018% and Cu0. 013%, the wolfram concentrate obtained by the flotation process above mentioned contains WO363.31% with recovery of 86.64% ,and sulfide concentrate contains Mo2.59% and Cul. 51% with recovery of 66.19% and 53.43% respectively. The flotation process can recovery tungsten, molybdenum and copper effectively.

关 键 词:黑钨矿 白钨矿 浮选 

分 类 号:TD952[矿业工程—选矿]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象