粉煤灰气相法制备纳米白炭黑研究  被引量:20

Study on preparing nanosized SiO_2·xH_2O from fly ash by gas-phase method

在线阅读下载全文

作  者:徐洁明[1] 谢吉民[1] 朱建军[1] 

机构地区:[1]江苏大学化学化工学院,江苏镇江212013

出  处:《无机盐工业》2006年第7期54-56,共3页Inorganic Chemicals Industry

基  金:江苏省"青蓝工程"基金项目(2001033);镇江市产学研基金项目(2005060)资助

摘  要:研究了利用粉煤灰与氟化钙等反应,用气相法直接制备纳米级SiO2·H2O的工艺条件。通过控制酸解和水解的速度,并在水解过程中加入乙醇作为分散剂,制备纳米白炭黑,借助红外光谱、XRD、TEM等技术对产物进行表征。结果表明,使用乙醇作为分散剂可以有效防止对纳米颗粒的团聚,制备出的白炭黑粒径可控制在10~20nm,纯度高达99.95%。The technological conditions of preparing nanosized SiO2 · xH20 from fly ash and calcium fluoride etc. by gas - phase method are studied. The preparation of SiO2 ·xH20 nanoparticle is carried out by controlling the speed of acid decomposing and hydrolyzing and by using ethanol as a dispersant during the hydrolyzing. The product is characterized by IR, XRD and TEM. The results show that it can prevent the nanoparticle from agglomeration when the ethanol as dispersant is used in the process. The size of SiO2·xH20 prepared can be controlled within 10 -20 nm and the purity of the product can reach 99.95%.

关 键 词:粉煤灰 气相法 纳米SIO2 白炭黑 

分 类 号:TQ127.2[化学工程—无机化工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象