异径轧制低碳钢的力学性能参数与粗糙度实验研究  

Experimental study on asymmetrical rolling with work roll edge contact

在线阅读下载全文

作  者:杨利梅[1] 姜正义 朱洪涛 刘相华[1] A.K.Tieu 

机构地区:[1]东北大学轧制技术及连轧自动化国家重点实验室,辽宁沈阳110004 [2]伍伦贡大学机械材料及机电一体化学院

出  处:《材料与冶金学报》2006年第3期208-211,共4页Journal of Materials and Metallurgy

基  金:澳大利亚联邦研究理事会创造发明基金(No.DP0211233);澳大利亚联邦研究理事会国际合作基金(No.LX0455066)

摘  要:通过一系列薄带异步轧制的实验,给出了压下率、轧制速度、轧件宽度及润滑条件等参数对轧制力和轧制力矩的影响.轧制力和轧制力矩随着轧件压下率、轧件宽度的增加而增加;轧制速度增加时,轧制力和轧制力矩降低;在轧件涂抹润滑剂的轧制条件下,轧制力和轧制力矩也降低.轧制完成后,薄带的表面粗糙度的值减少.同时也探讨了异径轧制过程中轧件表面的粗糙度的演变.In some cold rolling mills, edges of work rolls touch and deform when thin strip is rolled. Work roll edge contact forme a new deformation feature, especially for asymmetrical rolling of strip. In this paper, an experimental investigation has been carried out to study the effects of reduction, rolling speed, strip width and lubrication on the rolling force and torque during asymmetrical rolling of this strip with work roll edge contact. The rolling force and torque increases with the increasing of the reduction and the strip width. When the rolling speed is increased, the rolling force and torque decreases, and if lubricant is applied as a surface coating to the workpiece, the rolling force and torque also decrease. When the rolling is completed, the roughness of the strip surface is reduced. The surface roughness transfer during the special rolling is also discussed.

关 键 词:薄带钢 冷轧 异径轧制 

分 类 号:TG335.5[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象