磁性聚乳酸-羟基乙酸氧化酚砷纳米微粒的制备及其特性  被引量:2

Preparation and characterization of magnetic poly D,L-lactide-co-glycolide phenylarsine oxide nanoparticles

在线阅读下载全文

作  者:董勤[1] 蔡洪培[1] 张忠兵[1] 高申 

机构地区:[1]第二军医大学长征医院消化内科,上海200003 [2]药学院药剂学教研室,上海200433

出  处:《第二军医大学学报》2006年第12期1355-1357,共3页Academic Journal of Second Military Medical University

基  金:国家自然科学基金(30370644);上海科研计划项目(0352nm107).~~

摘  要:目的:研究磁性聚乳酸-羟基乙酸氧化酚砷纳米微粒(M-PLGA-PAO-NP)的制备工艺,并对纳米粒子进行评价。方法:运用超声乳化-溶剂挥发法制备磁性聚乳酸-羟基乙酸氧化酚砷纳米微粒,通过透射电镜(TEM)观察微粒形态,振动样品磁强计(VSM)确证纳米微粒磁性的存在,并对纳米微粒的平均粒径、载药量、包封率等进行评价。结果:纳米微粒外观呈规则球形,粒径在140~00nm占总数的80%,载药量为3.2%,包封率为34.2%,药物磁性较好。结论:获得了较满意的磁性聚乳酸-羟基乙酸氧化酚砷纳米微粒制备工艺,其过程简单,粒子性状符合要求。Objective: To study the preparation technique for magnetic poly D,L-lactide-co-glycolide phenylarsine oxide nanoparticles (M-PLGA-PAO-NPs) and to characterize the resultant product. Methods: M-PLGA-PAO-NPs were prepared by using emulsion-evaporation process. The morphology of the prepared nanoparticles were observed by transmission electron microscope and the magnetism of the particles was determined by vibrating sample magnetometer. Meanwhile, we also evaluated the mean diameter, encapsulation ratio, and drug loading rate of the particles. Results: The nanoparticles had a regular spherical surface, with 80% of them having a diameter of 140-500 nm. We also found that the drug loading rate of the particles was 3.2% and the mean encapsulation ratio was 34. 2%. The drug had satisfactory magnetic property. Conclusion: Our method can obtain M-PLGA-PAO-NP with satisfactory quality, it is simple-to-use and the prepared particles can meet the requirement of pharmaceutics.

关 键 词:氧化酚砷 聚乳酸-羟基乙酸 磁性 纳米粒 

分 类 号:R943.3[医药卫生—药剂学] R979.1[医药卫生—药学]

 