检索规则说明:AND代表“并且”;OR代表“或者”;NOT代表“不包含”;(注意必须大写,运算符两边需空一格)
检 索 范 例 :范例一: (K=图书馆学 OR K=情报学) AND A=范并思 范例二:J=计算机应用与软件 AND (U=C++ OR U=Basic) NOT M=Visual
作 者:汤慧萍[1] 刘海彦[1] 黄原平[1] 刘咏[2] 黄伯云[2]
机构地区:[1]西北有色金属研究院,陕西西安710016 [2]中南大学粉末冶金国家重点实验室,湖南长沙410083
出 处:《稀有金属材料与工程》2006年第12期1932-1935,共4页Rare Metal Materials and Engineering
基 金:国家"863"高技术项目(2001AA332010)
摘 要:研究了P/MTi-Mo合金中Mo对烧结致密化及力学性能的影响。用热膨胀仪分析了其收缩/膨胀特性,用扫描电镜及力学性能检测等分析手段研究了显微组织和力学性能。结果表明,Mo的添加不利于P/MTi-Mo合金的烧结致密化,但有利于Ti-Mo合金的显微组织细化。随着Mo含量的增加,组织细化作用更加明显。该晶粒细化作用大大改善了合金的室温塑性,使烧结态Ti-Mo合金的延伸率达到23%。The effects of molybdenum addition on the sintering densification and mechanic properties of Ti-Mo alloy were investigated. The expansion/shrinkage characteristic of the alloy was analyzed by a dilatometer. The microstructure and mechanical properties of the alloy were studied by SEM and mechanical property measurement and test. The results show that the addition of Mo can't accelerate the sintering densification, but is beneficial to microstructure refining of Ti-Mo alloy. With increasing of Mo content, the microstructure refming is more and more obvious, resulting in great improving the ambient temperature plasticity of the alloy, the elongation of as-sintered Ti-Mo alloy can reach 23%.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.3