出 处:《稀有金属材料与工程》1996年第6期36-39,共4页Rare Metal Materials and Engineering
摘 要:研究了配碳量与Ni/Co比对WC-9(Ni-Co)硬质合金抗弯强度的影响。实验结果表明:WC-3Ni-6Co的配碳量是6.04wt%时,其抗弯强度与WC-9Co硬质合金相当;Ni的分布均匀性对抗弯强度的影响极其重要,粗粒Ni粉或(和)较多η相的存在都会使硬质合金形成脆性断裂,直接影响合金的抗弯强度。he effect of carbon content and the Ni/ Co ratio in WC-9(Ni-Co) alloy on transverse rupture is investigated systematically. The results show that the transverse rupture strength of WC-3Ni-6Co alloy is equal to that of WC-9Co alloy as the carbon content of WC-3Ni-6Co is adjusted to about 6.04 wt%. It is also show that the effect of the distributive homogeneity of Ni powder on the transverse rupture strengthis very important. Coarse Ni powder and the existence of more η-phase result in the brittle rupture of the carbide and affect directly the transverse rupture strength of the carbide.
分 类 号:TG135.5[一般工业技术—材料科学与工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.31