浅析加氢精制喷气燃料银片腐蚀的影响因素  被引量:3

An Analysis of the Influencing Factors in Sliver Strip Corrosion in Hydrogenated Jet Fuel

在线阅读下载全文

作  者:刘勇华 安建勇[2] 申士强[3] 

机构地区:[1]驻中石化广州分公司军代室,广州510726 [2]后勤工程学院训练部,重庆400016 [3]驻中石化天津分公司军代室,天津300271

出  处:《后勤工程学院学报》2007年第1期38-40,44,共4页Journal of Logistical Engineering University

摘  要:硫化氢和元素硫是直接造成加氢精制生产过程中银片腐蚀不合格的物质。从生产环节入手,对汽提效果、非计划停工、原料性质、水、生产设备对3号喷气燃料银片腐蚀的影响进行了分析,并对生产中存在的问题提出了用精制油代替粗汽油作冷回流介质,用氢气代替水蒸气作汽提介质等整改措施。Hydrogen sulfide and dement sulfur are the main materials which directly cuase the unqualification of silver strip corrosion during jet fuel hydrotreating. The influencing factors , such as stripping tower effect, non - plan shutting down, raw materials properties, water and production equipments, are analyzed. In this paper, methods guaranteeing qualification of silver strip corrosion,including using jet fuel instead gasoline as cooling medium, using hydrogen instead vapour as stripping medium, are put forward.

关 键 词:喷气燃料 加氢精制 银片腐蚀 影响因素 

分 类 号:TE626.23[石油与天然气工程—油气加工工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象