作 者:李代叙[1] 雷军[1] 周海英[1] 申开智[1]
机构地区:[1]四川大学高分子科学与工程学院高分子材料工程国家重点实验室
出 处:《现代塑料加工应用》2007年第1期12-15,共4页Modern Plastics Processing and Applications
基 金:国家自然科学基金(基金号10590352)
摘 要:高密度聚乙烯/茂金属线性低密度聚乙烯(HDPE/mLLDPE)40/60共混物经混炼器混炼后的冲击强度比未经混炼器混炼的HDPE增加了96.2%,比未经混炼器混炼的mLLDPE增加了27.0%,其拉伸强度比未经混炼器的mLLDPE增加了49.1%。这表明在混炼器的强剪切分散作用下,HDPE,mLLDPE共混对HDPE和mLLDPE有显著的增韧作用。其微观结构测试表明,mLLDPE与HDPE形成了共晶结构,HDPE含量高的HDPE/mLLDPE共混体系试样内部的晶粒尺寸更为均一。The impact strength of HDPE/mLLDPE 40/60 blends compounded with mixer, is enhanced by 96. 2% compared with pure HDPE and 27% compared with mLLDPE. In the meantime, the tensile strength of the blends is enhanced by 49. 1% compared with pure mLLDPE. The results show that mixer with intensive shear and disperse cause toughen effect of the blends. Through the investigation of micro-structure, it is found that co-crystals structure of HDPE and mLLDPE forms in the blends. In addition, it can be seen that the size of crystal is more uniform when HDPE content is high.
关 键 词:高密度聚乙烯 茂金属聚乙烯 共混 混炼器 转速 共晶
分 类 号:TQ325.12[化学工程—合成树脂塑料工业]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.7