鞍钢3号高炉氧煤强化炼铁工业试验  被引量:4

Industrial experiment of intensified smelting by oxygen-coal injection on No. 3 BF of Anshan Iron & Steel Group Co.

在线阅读下载全文

作  者:林滋泉[1]  

机构地区:[1]鞍山钢铁集团公司

出  处:《炼铁》1997年第1期1-4,共4页Ironmaking

摘  要:1995年8月21日~11月20日在鞍钢3号高炉(831m^3)进行了煤比为200kg/t的氧煤强化炼铁工业试验。试验达到了预期目标,煤比平均达203kg/t,富氧率3.42%,煤焦置换比0.8,实现了低富氧率条件下高煤比的强化冶炼。An industrial experiment of intensified smelting by, oxygen-coal injection with coal injection rate of 200 kg/tHM was carried out on No. 3 BF (831m3) of Anshan Iron & Steel Group Co. from August 21 to November 20,1995. The results obtained for three months in succession are as follows:average coal injection rate is more than 203 kg/tHM,oxygen enrichment rate is 3.42%, coal-to-coke replacement ratio is 0.8. The expected experiment goal had been attained and the intensified smelting with low oxygen enrichment rate and high coal injection rate had been achieved.

关 键 词:高炉 强化冶炼 氧煤喷吹 工业试验 

分 类 号:TF538[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象