济钢1~#1 750m^3高炉降低渣中Al_2O_3含量的操作实践  被引量:1

Operational Practice of Reducing the Al_2O_3 Content of the Slag of No.1 1 750 m^3 BF in Jigang

在线阅读下载全文

作  者:李传辉[1] 潘协田[1] 冯增铭[1] 

机构地区:[1]济南钢铁股份有限公司第一炼铁厂,山东济南250101

出  处:《山东冶金》2007年第3期13-14,共2页Shandong Metallurgy

摘  要:针对1#1750m3高炉渣中Al2O3含量高,使炉渣黏稠,影响高炉顺行的情况,通过加辅料,成功地控制渣中Al2O3小于16%,保持了炉料结构相对稳定,改善了高炉操作技术指标,加辅料后的第2月,利用系数达2.538t/(m·3d),入炉焦比为346kg/t。Because of the Al2O3 content of the slag of No.1 1 750 m^3 BF in Jigang was high, making the slag sticky and effecting regular blast-furnace performance, auxiliary materials were added. Then the Al2O3 content of the slag was controlled less than 16% triumphantly. Burden design was stabilized relatively. The operational indexes of blast furnace were improved well. Furnace productivity reached 2.538 t/(m^3·d) and coke ratio reached 346 kg/t in second month after adding auxiliary material.

关 键 词:高炉 炉渣 Al2O3含量 操作实践 

分 类 号:TF534[冶金工程—钢铁冶金]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象