出 处:《铝加工》2007年第4期14-17,共4页Aluminium Fabrication
摘 要:简明扼要地分析了铝铸轧辊辊套内外表面的温度变化及辊套内热应力的形成及其变化规律,着重论述了辊套表面热裂纹的形成与扩展,提出了修正辊套表面热裂纹的措施及合理选择抗热疲劳辊套材料的要求,认为32Cr3Mo1V钢是一种较好的抗热疲劳裂纹的辊套专用材料。The temperature changes in the outside and inside surface of aluminum cast - rolling roller shell, the formation of thermal stress in shell and the regularity of change were briefly described in the paper. The formation and extension of cracks on shell surface were addressed in some detail, and the countermeasures and requirements for proper choice of shell material with thermal fatigue resis- tence were set forward as well as. 32Cr3MolV steel is regarded as a good material for roller shell.
关 键 词:铝铸轧辊辊套 温度梯度 热应力 热疲劳裂纹 辊套材料
分 类 号:TG113.255[金属学及工艺—物理冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.15