作 者:周世祥[1] 许诚信[1] 屠宝洪[1] 华建民[2] 许文清[2]
机构地区:[1]北京科技大学冶金学院,北京100083 [2]江苏锡钢集团公司,无锡214026
出 处:《北京科技大学学报》1997年第4期338-341,共4页Journal of University of Science and Technology Beijing
摘 要:叙述了用铝渣灰脱硫剂提高脱硫效果缩短LF炉处理时间的试验,着重分析了此脱硫剂的脱硫效果和影响因素核试验的工艺要点是:控制好顶渣成分,提前造渣,钢液脱氧良好,增加吹氩强度.结果表明,用含铝渣灰的脱硫剂处理钢水,当每t钢加入量为15~20kg时,LF炉处理时间平均缩短10min,平均脱硫率提高16%.The experiments using synthetic desulphurizer with Aluminum slag ash toincrease the efficiency of desulphurization and shorten the LF process time were described.The efficiency of mis desulphurizer and factors influencing its effects were emphaticallyanalysed. The gists of the experiments process were as follows: the optimum control oftop slag composition, forming the top slag in ladle eariy, the good deoxidation,increasing the Ar gas shtring strength. The experimental results showed that given thedesulphurizers addition among 15~ 20 kg/t, the average LF process time is shorted 10Ann, the average desulpherizing rate is raised 16 %.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.3