非晶态NiMoAl合金催化葡萄糖加氢制备山梨醇  被引量:7

Hydrogenation of Glucose to Sorbitol over Amorphous NiMoAl Alloys Catalyst

在线阅读下载全文

作  者:杜文强[1] 王越[1] 吕连海[1] 

机构地区:[1]大连理工大学化工学院精细化工国家重点实验室,辽宁大连116012

出  处:《精细化工》2007年第12期1204-1206,共3页Fine Chemicals

基  金:辽宁省自然科学基金资助项目(20052188)~~

摘  要:研究了非晶态NiMoAl在葡萄糖加氢制备山梨醇反应中的催化性能,考察了反应温度、压力和催化剂用量对反应的影响,并与5种钼改性骨架镍催化剂作了活性比较。结果表明,采用质量分数50%的葡萄糖水溶液,非晶态NiMoAl为催化剂,在温度135℃,压力4.0MPa下,原料100%转化,山梨醇选择性大于99%,催化剂连续套用5次,活性保持不变。The amorphous NiMoAl alloy catalyst was used in liquid phase selective hydrogenation of glucose to sorbitol. The effects of various reaction parameters like reaction temperature, pressure and amount of catalyst were investigated, and the activities of five different kinds of Mo modified skeletal catalysts were compared. The results show that glucose in equivalent amount of water can be 100% converted with more than 99% selectivity to sorbitol at 135 ℃and 4.0 MPa pressure by the amorphous NiMoA1 alloy catalyst. The catalyst can be repeatedly used for five times, indicating excellent stability.

关 键 词:葡萄糖 山梨醇 非晶态NiMoAl 加氢 

分 类 号:TQ032.4[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象