无熟料矿渣粉煤灰胶凝材料强度影响因素研究  被引量:8

Research on strength influencing factor of slag-fly ash cementitious material without clinker

在线阅读下载全文

作  者:王薇[1] 倪文[1] 张旭芳[1] 刘凤梅[1] 余佳[1] 

机构地区:[1]北京科技大学金属矿山高效开采与安全教育部重点实验室,北京100083

出  处:《新型建筑材料》2007年第12期8-11,共4页New Building Materials

基  金:国家科技支撑计划课题资助(2006BAC21B03)

摘  要:针对矿渣、粉煤灰的成分及特点,研制了一种无熟料矿渣粉煤灰胶凝材料,并对其强度影响因素、水化性能进行了研究。结果表明,加入70%矿渣,15%粉煤灰,10%石膏,5%复合激发剂,可以制备性能较好的胶凝材料,28d抗压强度可达到58.21MPa。According to composition and features of slag and fly ash,the cementitious material without clinker has been made and its strength influencing factors and the hydration capability have been studied. The results are as follows:the high-strength cementitious material can be made by adding 70 percent of slag, 15 percent of fly ash, 10 percent of gypsum and 5 percent of complex activated material and the compression strength at 28 d is up to 52.81 MPa.

关 键 词:矿渣 粉煤灰 复合激发剂 胶凝材料 

分 类 号:TU528[建筑科学—建筑技术科学]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象