机构地区:[1]丽水学院机械电子与建筑工程学院,浙江丽水323000 [2]浙江工业大学建筑工程学院,浙江杭州310014
出 处:《丽水学院学报》2008年第2期46-48,共3页Journal of Lishui University
摘 要:分别通过对3个不同水灰比(0.25,0.30,0.35)和4个不同养护温度(10℃,20℃,30℃,40℃)条件下28d龄期内水泥胶砂自收缩的测定,揭示了水泥胶砂自收缩与养护温度之间的依存关系,为高强混凝土自收缩温度依存性的后续研究提供必要的参考依据。得出同一水灰比的胶砂,随着养护温度的升高,早龄期自收缩速率加快,自收缩量明显增大;随着水灰比的降低,自收缩量显著增大等初步结论。For the purpose of exposing the relationship between autogenous shrinkage of high strength mortar(HSM)and its curing temperature, a survey has been performed on autogenous shrinkage of HSM with three different water cement ratios( W/C ) (0.25,0.30,0. 35) by four different curing temperatures (10℃, 20℃, 30℃, 40℃) in initial 28d age. Maybe, it can offer some essential reference for further research on temperature dependence of autogenous shrinkage of HSC/HPC. The conclusion is obtained that with the rising of curing temperature of mortar with a certain w/c, the rate and total amount of autogenous shrinkage strain increases promptly in early age, and with decreasing of w/c, the autogenous shrinkage strain increases apparently.
分 类 号:TB302.3[一般工业技术—材料科学与工程]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.28