摘  要:顺序共注射模塑中的芯层熔体前沿冲破是造成共注制品报废的重要原因之一,合理控制壳层预填充量可预防此现象发生。从运动学角度探讨芯层熔体冲破的影响因素,建立预测最小壳层预填充量的方程,并在Moldflow平台上进行验证。The core-melt breakthrough is one of the most important reasons that a waster is produced in the sequential co-injection molding, which could be prevented by controlling properly pre-iilled polymer volume fraction. Through the view of kinematics, discussed the reasons that affect the core-melt breakthrough, and created a mathematic formula for forecasting min pre-filled polymer volume fraction. Then validated above conclusion by the Moldflow software.

关 键 词:顺序共注成型 壳层预填充量 芯层熔体前沿冲破 数值模拟 

分 类 号:TQ320.1[化学工程—合成树脂塑料工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象