机构地区:[1]南昌大学材料科学与工程学院,江西南昌330031 [2]中国工程物理研究院,四川绵阳621000
出 处:《功能材料》2008年第7期1099-1101,共3页Journal of Functional Materials
基 金:国家自然科学基金--NSAF联合基金资助项目(10576014)
摘 要:采用4284A阻抗分析仪,在0-1MHz频率范围内,研究了不同测试温度和退火条件下硅橡胶表面状态的非晶Fe73.5Cu1Nb3Si13.5B9带材的压磁性能。结果表明,非晶带材的阻抗变化|ΔZ|随着压应力和频率的增加而增加,对0.1MPa以下的微应力变化非常敏感;在13-37℃测试温度范围内,随着温度的升高,非晶带材压磁灵敏度增加,37℃时压磁性能最好;退火温度低于300℃时,非晶带材经300℃×0.5h退火处理后,其压磁性能最好。The effect of annealing process and testing temperature on piezomagnetic properties of amorphous Fe73.5Cu1Nb3 Si13.5B9 strips that surface covered silicon rubber are studied in the frequency range of 0Hz-1MHz by 4284A impedance analyzer. The results show that |ΔZ| of amorphous strips increase as stress and frequency increase, the amorphous strips are very sensitive when stress change from 0MPa to 0.1MPa; When testing temperatures are in the range from 13-37℃, sensitivity of piezomagnetic properties increase as temperature increase, especially in 37℃ The piezomagnetic properties of amorphous strips are the best at 300℃ for 0.5h when annealing temperatures under 300℃.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:18.224.72.117