作 者:肖大玲[1] 赵秀英[1] 向平[1] 刘俊杰[2] 张立群[1,2]
机构地区:[1]北京化工大学北京市新型高分子材料制备与加工重点实验室,北京100029 [2]北京化工大学纳米材料先进制备技术与应用科学教育部重点实验室,北京100029
出 处:《橡胶工业》2008年第11期660-664,共5页China Rubber Industry
摘 要:采用熔融共混法制备受阻酚AO-80/聚酯型热塑性聚氨酯(PES-TPU)复合材料,并对其性能进行研究。结果表明,受阻酚AO-80/PES-TPU复合材料中,受阻酚AO-80呈无定形态,与PES-TPU基体的相容性良好;随着受阻酚AO-80用量的增大,受阻酚AO-80/PES-TPU复合材料的损耗因子峰值增大,损耗峰向高温方向移动,阻尼性能提高,但拉伸性能有所降低。A hindered phenol AO-80/polyester-based polyurethane thermoplastic elastomer(PESTPU) composite was prepared by melt blending, and its properties were investigated. The results showed that the hindered phenol AO-80 showed amorphous state in the hindered phenol AO-80/PES- TPU composite,and the compatibility between hindered phenol AO-80 and PES-TPU was good;the peak value of rand of hindered phenol AO-80/PES-TPU composite increased, the peak position of tanδ moved to higher temperature zone, and the damping property of the composite was improved, but the tensile properties reduced as the addition level of hindered phenol AO-80 increased.
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:216.73.216.81