丁腈橡胶/氯化丁基橡胶共混物的性能研究  被引量:2

Study on the properties of NBR/CIIR blend

在线阅读下载全文

作  者:李俊[1] 董丽杰[1] 舒本勤[1] 潘民选[1] 刘景涛[1] 李蕊[1] 

机构地区:[1]武汉理工大学材料学院,湖北武汉430070

出  处:《弹性体》2008年第6期28-30,共3页China Elastomerics

摘  要:研究了丁腈橡胶/氯化丁基橡胶共混物的低温性能和耐热性能。结果表明,选用TMTD/ CZ/ZnO作共硫化体系,共混物体系两相的相容性较好;在并用比例为70/30时,与纯NBR相比,共混物Tg下降5.5℃,失重5%热分解温度提高38.4℃,且耐油性变化很小,适宜制备高低温性能较好的耐油橡胶制品。The low temperature performance and heat resistance of NBR/CIIR blend were investi- gated. The result showed that the two phases in blend exhibited good compatibility when adopting TMTD/CZ/ZnO vulcanization system. As the blending ratio of NBR/CIIR was 70/30, Tg decreased by 5.5 ℃ ,and 5% thermal decomposition temperature increased hy 38.4℃. Moreover, the oil resistance changed a little. The blend was suitable for manufacturing oil resistance rubber products requiring better high and low-temperalure performances.

关 键 词:丁腈橡胶 氯化丁基橡胶 共混物 性能 

分 类 号:TQ333.7[化学工程—橡胶工业] TQ333.6

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象