高分辨热敏微胶囊信息材料及其影像特性  被引量:3

Heat sensitive microcapsule as high resolution information materials and its image property

在线阅读下载全文

作  者:李晓苇[1] 任少波[1] 赖伟东[1] 孟双双[1] 张楠[1] 傅广生[1] 

机构地区:[1]河北大学物理科学与技术学院,河北保定071002

出  处:《分子科学学报》2008年第6期433-435,共3页Journal of Molecular Science

基  金:河北省自然科学基金资助项目(E2005000131);高等学校博士学科点专项科研基金资助项目(20060075003);教育部科学技术研究重点资金项目(207147)

摘  要:利用界面聚合法制备了亚微米级染料前体微胶囊和显色剂微胶囊,探讨了显影条件、囊壁材料用量与影像密度之间的关系.分析表明显影温度、显影时间、囊壁材料用量共同影响影像密度,显影温度决定了囊壁的渗透能力,显影时间决定了显色反应程度,而囊壁材料用量决定了囊壁厚度进而影响影像密度.得到最佳显影温度区间为130℃-140℃,最佳显影时间为5s.The interface-polymerization method was applied to fabricate the submicrometer structure dye precursor microcapsules and developer microcapsules. The relationship between developing conditions and image density, as well as the weight of microcapsule wall material and image density were obtained. The analysis indicated that the image density could be affected by developing temperature, developing time and the weight of microeapsule wall material. Developing temperature determined the penetration ability of microcapsule wall. Developing time determined the image formation degree. The weights of mierocapsule wall material determined the thickness of mierocapsule wall and developing density. The optimal range of developing temperature was 110 ℃ - 140 ℃ and the optimal developing time was 5 s.

关 键 词:热敏微胶囊 影像密度 显影温度 显影时间 囊壁 

分 类 号:TQ314[化学工程—高聚物工业]

 