作 者:张发明[1] 林日孝[1] 曾庆军[1] 张先华[1]
机构地区:[1]广州有色金属研究院
出 处:《金属矿山》2009年第1期85-88,共4页Metal Mine
摘 要:根据原矿的矿石性质,试验研究了钼铋混浮-精矿钼铋分离-尾矿重选回收钨的选矿工艺流程。对含钼0.24%、铋0.10%、钨(WO3)0.052%的原矿,获得了含钼52.43%、钼回收率92.15%的钼精矿;含铋37.09%、回收率75.60%的铋精矿,含铋1.85%、回收率12.16%的铋中矿、铋总回收率87.76%及含钨(WO3)65.24%、钨回收率58.22%的钨精矿。钼、铋、钨均得到有效回收。In light of the properties of the run-of-mine ore, a beneficiation process of molybdenite and bismuthinite bulk flotation- molybdenite and bismuthinite separation-wolframite recovery from tailings was tested. As a result, from a feed containing Mo 0.24%, Bi 0.10% and WO3 0.052%, the following products were obtained, including a molybdenite concentrate grading 52.43% Mo at a recovery of 92.15%, a bismuthinite concentrate grading 37.09% Bi at a recovery of 75. 60% , and sub-bismuthinite concentrate grading 1.85% Bi at a recovery of 12.16% , with a total Bi recovery of 87.76% ; and a wolframite concentrate grading 65.24% WO3 at a recovery of 58.22% , achieving a good recovery of Mo, Bi and WO3.
分 类 号:TD952[矿业工程—选矿] TF817.032[冶金工程—有色金属冶金]
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在载入数据...
正在链接到云南高校图书馆文献保障联盟下载...
云南高校图书馆联盟文献共享服务平台 版权所有©
您的IP:18.191.149.30