石墨插层化合物的微波法制备工艺研究  被引量:3

Research on Preparation and Graphite Intercalation Compound by Micro-wave Bulking

在线阅读下载全文

作  者:马烽[1] 杨晓勇[1] 程立媛[1] 

机构地区:[1]山东轻工业学院化学工程学院,济南250353

出  处:《材料导报(纳米与新材料专辑)》2008年第3期253-255,共3页

基  金:山东省自然科学基金(Y2005F12)

摘  要:以浓硫酸为插入剂,高锰酸钾为氧化剂用化学方法制备出石墨插层化合物,并用微波进行了膨化。通过正交实验优化了制备工艺影响因素,得出了各因素对膨化率由强到弱的影响次序:反应时间,微波功率,H_2SO_4(g)用量,KMnO_4(g)用量。确定出最佳影响因素水平:反应时间1h,微波功率800W,H_2SO_4用量50g,KMnO_4用量4g。膨胀体积可以达到约400mL/g。并用XRD和EDS等技术对样品进行了表征。Using sulfuracid as intercalation agent and potassium permanganate as oxidizer, the graphite intercalation compound is prepared by electrochemical method and is bulked in micro-wave oven. Reaction conditions are optimized by using orthogonal design, and the sequence of factors influencing the ratio of expansion is obtained, which was, from strong to weak, the reaction time, the power of micro-wave, the sulfuracid amount and the potassium permanganate amount. The optimum technical parameters were determined, namely, the reaction time 1h, the power of micro-wave 800W, the amount of sulfuracid 50g, the amount of potassium permanganate 4g. The largest expanding volume is 400mL/g. The graphite intercalation compound is characterized and analyzed by XRD and EDS techniques.

关 键 词:可膨胀石墨 化学氧化法 微波 

分 类 号:TQ165[化学工程—高温制品工业] TQ424.25

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象