热轧平整压力导致厚度不合的分析与对策  

Analysis on gauge deviation due to flattening force difference and countermeasures

在线阅读下载全文

作  者:毕士龙[1] 张斌[1] 周一中[2] 程小勇[1] 周学俊[3] 

机构地区:[1]武钢股份公司质检中心,湖北武汉430083 [2]武钢股份公司热轧厂,湖北武汉430083 [3]武钢股份公司生产技术部,湖北武汉430083

出  处:《武钢技术》2009年第2期18-19,33,共3页Wisco Technology

摘  要:某热轧厂平整线生产热轧商品材SPHT2,连续发生厚度不合9卷,造成批量性尺寸改判。通过现场生产情况的排查,重新模拟当时的生产过程,发现此批量性厚度不合的现象,与该机组的平整辊压力有密切关系。通过分析计算,得出平整线压力与厚度、宽度变化的一般方程。对今后热轧卷的尺寸把关起到重要的预警作用。9 of commercial coils SPHT2 produced on the leveling line of a specific hot rolled mill happened to be differential in depth consecutively leading to dimension reclassification of a whole batch. By way of check and examination on-site and simulation of the production conditions it's discovered that the deviation of thickness of the batch relates to the pressure of flattening rolls. Through analysis and calculation the universal equation of relations between pressure of flattening rolls, depth and width is derived. It is of great importance in forecasting coils dimension.

关 键 词:热轧平整 厚度不合 平整压力 尺寸把关 

分 类 号:TG335.11[金属学及工艺—金属压力加工]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象