脆化温度对粘土再生砂微粉去除率的影响  被引量:1

Effect of Brittle Temperature on Micro Powder Removal Ratio of Reclaimed Green Sand

在线阅读下载全文

作  者:孙清洲[1] 张普庆[1] 赵中魁[1] 张艳[1] 

机构地区:[1]山东建筑大学材料科学与工程学院,山东济南250101

出  处:《铸造》2009年第4期394-396,共3页Foundry

基  金:山东省科技攻关项目(2005GG3206092);山东省自然科学基金项目(Y2006F28)

摘  要:对粘土砂再生前的脆化温度进行了试验研究,发现在相同的再生机和负压流化床工作参数下,对粘土砂进行烘干后再生所获再生砂的微粉去除率最低,经高温脆化后再生所获再生砂的微粉去除率最高。采用700℃高温脆化时,随保温时间的延长,再生砂的微粉去除率提高,当保温10min,然后再进行机械再生及去除微粉操作时,可以获得泥分含量低于同种新砂的再生砂,并且再生粘土砂的微粉去除率随再生次数的增加而提高。Brittle temperature of green sand before reclamation was studied. When the work conditions of the reclaimer and vacuum fluidized bed are identical, the removal ratio of micro powder for the reclaimed sand by drying is the lowest and that by high temperature embrittlement is the highest. When embrittling at 700 ℃, the longer the holding time, the higher the removal ratio of micro powder of the reclaimed sand. With 10 min holding time, mechanically reclaiming and removing micro powder by vacuum fluidized bed, micro powder content of the reclaimed sand is lower than the new sand. The removal ratio of micro powder of the reclaimed sand increases with increasing reclamation times.

关 键 词:粘土砂 再生 脆化 微粉去除率 

分 类 号:TG221[金属学及工艺—铸造]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象