含砷飞灰固化处理研究  被引量:4

Solidification Treatment of Arsenic-containing Fly Ashes

在线阅读下载全文

作  者:蔡忠林[1] 庞敏晖[2,3] 李善茂[2] 汪吉章[2] 王鑫[2] 李伟[2] 

机构地区:[1]中国人民解放军73921部队 [2]防化指挥工程学院分析中心 [3]中国人民解放军95863部队

出  处:《安全与环境工程》2009年第3期62-65,69,共5页Safety and Environmental Engineering

摘  要:通过试验确定了胶凝材料的组成体系,探讨了影响胶凝材料性能的主要工艺参数,确立的最佳固化工艺条件为:水泥∶砂子∶飞灰=57.6∶40∶2.4,水灰比为0.28,水泥采用标号为42.5的快硬硫铝酸盐特种水泥,以硫化钠作为添加剂,其用量为飞灰/硫化钠=1.5。在最佳配比和最佳养护条件下,固化体在实验室条件下抗压强度可达2.5 MPa,砷的浸出浓度为0.83 mg/L,达到了相关的填埋标准。This paper investigates the component system and the different factors which influence the properties of the cementing materials, and then makes a conclusion that the optimum solidification conditions are as follows: the ratio of cement, sand and fly ash is 57.6 : 40 : 2.4,the proportion of water and solid is 0.28, the tab of specific cement is 42.5, and the proportion of fly ash and sulfureted sodium is 1.5. The compressive strength of the solidified body in the lab is 2.5 MPa and the leaching concentrations of arsenic is 0.81 mg/L, so the properties can reach the corresponding criteria of the fill.

关 键 词: 飞灰 固化/稳定化 

分 类 号:X701[环境科学与工程—环境工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象