高温耐磨蚀涂层防护技术在热电偶保护套管上的应用  被引量:4

The Application of High Temperature Wear and Corrosion Protection Coating Technology in Thermocouple Cannula

在线阅读下载全文

作  者:李伟 王灿明[2] 渠智彦[2] 毕继鑫[2] 

机构地区:[1]兖矿科奥铝业有限公司济三电厂,山东济宁272000 [2]山东科技大学材料学院,山东青岛266510

出  处:《中国仪器仪表》2009年第5期85-88,共4页China Instrumentation

摘  要:针对热电偶保护套管在使用过程中存在的高温腐蚀与磨损现象,介绍了两种新的表面防护涂层。采用电弧喷涂技术制备出Cr3C2/B-Fe金属/陶瓷涂层,采用热喷涂+高温冶金反应法制备出Fe(Ni)-Al系金属间化合物涂层。采用上述涂层保护的热电偶保护套管,在循环流化床锅炉中应用,使用寿命长达9~12个月,取得了较好的效果。In this article, new surface coating protection processes was introduced according to the wear and corrosion mechanism of thermocouple cannula at high temperature. Cr3C2/B-Fe metal/ceramic coating was prepared by arc spraying technology and Fe(Ni)-A1 series intermetallic compound coating were prepared by thermal spray + heat metallurgical reaction method. The service life of thermocouple cannula protected by such coatings is up to 9 to 12 months.

关 键 词:热电偶保护套管 金属间化合物 涂层 耐磨 耐蚀 

分 类 号:TG174.4[金属学及工艺—金属表面处理]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象