黑龙江配煤制备活性炭的工艺研究  被引量:4

Preparation process of activated carbon with Heilongjiang blended coal

在线阅读下载全文

作  者:邵景景[1] 高丹[2] 薛红艳[1] 熊楚安[1] 徐革联[1] 

机构地区:[1]黑龙江科技学院资源与环境工程学院,黑龙江哈尔滨150027 [2]黑龙江科技学院图书馆,黑龙江哈尔滨150027

出  处:《洁净煤技术》2009年第4期83-86,共4页Clean Coal Technology

基  金:黑龙江教育厅科学技术研究项目:黑龙江省配煤制备高比表面煤基活性炭的研究(11531328)

摘  要:为寻求黑龙江煤制备高比表面活性炭的适宜原料配比及工艺条件,以七台河煤与依兰煤配煤制备活性炭,用正交实验法,考察原料煤配比、碱炭比、活化温度、活化时间等因素对活性炭碘吸附值的影响,获得了最适宜工艺条件:七台河煤与依兰煤配比1/1,碱炭比6/1,活化温度850℃,炭活化时间120min。在此条件下所得活性炭的碘吸附值可达1973mg·g^-1,比表面达1735m^2·g^-1。对于拓宽黑龙江煤炭应用领域具有一定的现实意义。In order to find optimal raw material ratio and preparation process of HSAAC (high surface area activated carbon) with Heilongjiang coal , studied preparation of activated carbon by blended coal from Qitaihe and Yilan, the factors of the absorption value of I2, such as ratio mixture of coals, ratio of alkali to carbon, activated tempera- ture, activated time by the method of orthogonal design. The study features the best condition: Qitaihe and Yilan coal ratio 1, alkali-carbon ratio 6, activated temperature 850℃, activated time 120min. In this condition the absorption value of I2 and BET surface area respectively reached up to 1973mg·g^-1 and 1735m^2·g^-1. This disquisition has definite practical significance for open the applied realm of Heilongjiang coal.

关 键 词:活性炭 炭活化反应 配煤 

分 类 号:TQ424.11[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象