测压钻孔三相泡沫密封液的试验研究  被引量:3

Experimental Investigation of Three-phase Foam Sealing Liquid for Gas Pressure Determination Borehole

在线阅读下载全文

作  者:禹东方[1] 陈学习[2] 马尚权[2] 柏松[2] 

机构地区:[1]北京大学 [2]华北科技学院

出  处:《金属矿山》2009年第9期165-168,共4页Metal Mine

基  金:国家重点基础研究"973"项目(编号:2005cb221504);国家"十一五"科技攻关项目(编号:2006BAK03B01)

摘  要:为选择合适的封堵钻孔裂隙三相泡沫,通过对3种发泡剂、4种稳泡剂和3种不同粒径范围固相填充物的试验研究,得出了发泡倍数高、稳定时间长和携带固体物能力强的三相泡沫密封液材料配比,即:水溶液质量比0.4%的发泡剂FP-1、1%的稳泡剂WP-3和4%的粒径范围0.2-1 mm的混合固相填充物。现场应用试验表明,该材料配比的三相泡沫封堵测压钻孔裂隙,具有封孔时间短、测定过程快、测定值准确性高等特点,对提高瓦斯压力测定水平具有重要意义。In order to select suitable three-phase foam for sealing fracture around borehole,3 kinds of foam agents,4 kinds of stabilizing agents and 3 kinds of solid-phase filler with different particle diameter were studied. Three-phase foam sealing liquid proportion with high foamability, good stability and strong ability of carrying solid was obtained. The proportion is : 0.4 percent of foam agent FP-1,1 percent of stabilizing agent WP-3 and 4 percent of mixed solid-phase filler with 0.2 to 1 mm diameter. Practical application shows that this proportional three-phase foam has characteristics of little sealing bore- hole time, rapid determination process and high determination accuracy, which is meaningful for raising the level of gas determination.

关 键 词:测压钻孔 三相泡沫 泡沫性能 材料配比 

分 类 号:TQ637.8[化学工程—精细化工] TE358.3[石油与天然气工程—油气田开发工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象