凹凸棒石黏土脱色剂对碳九馏分进行脱色  被引量:4

Decolorization of C_9 fraction with attapulgite clay decolorant

在线阅读下载全文

作  者:宗绪伟[1] 王青宁[1] 姜瑞雨[1] 叶业通[2] 李澜[1] 

机构地区:[1]兰州理工大学石油化工学院,甘肃兰州730050 [2]兰州理工大学机电工程学院,甘肃兰州730050

出  处:《化工进展》2009年第11期1969-1973,共5页Chemical Industry and Engineering Progress

基  金:甘肃省攻关基金项目(2GSO47-A52-001-05)

摘  要:以甘肃临泽凹凸棒石黏土为载体,MnO2为活性剂,制备脱色剂对碳九(C9)馏分进行脱色。通过正交实验研究了酸度、焙烧温度、活性组分加入量、脱色剂的用量和脱色时间对C9馏分脱色的影响。结果表明,焙烧温度600℃、活化浓度6%、活性组分MnO2含量4%、脱色剂用量8g、脱色时间在60min时,能够使C9馏分的脱色率达到78.66%。Attapulgite clay decolorant was prepared for the decolorization of C9 fraction. Effects of sulphuric acid, calcination temperattre, active component, amount of decolorant and decoloring time on the decolorization of C9 fraction were investigated. Results showed that the decolorant, which was prepared from attapulgite clay treated with 6% sulphuric acid calcinated at 600℃ with the addition of 4% MnO2, has the best decolorization efficiency, and the decolorization rate of C9 fraction can be achieved up to 78.66%.

关 键 词:凹凸棒石黏土 C9馏分 脱色剂 吸附 

分 类 号:TE624.54[石油与天然气工程—油气加工工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象