用于松香氢化的失活催化剂Ni/Al_2O_3-M_xO_y的再生研究  

Study on Regeneration of the Deactivated Catalyst Ni/Al_2O_3-M_xO_y Used for Hydrogenation of Gum Rosin

在线阅读下载全文

作  者:蒋丽红[1] 王亚明[1] 史晓杰[1] 

机构地区:[1]昆明理工大学化学工程学院,云南昆明650224

出  处:《林产化学与工业》2009年第B10期159-164,共6页Chemistry and Industry of Forest Products

基  金:云南省应用基础研究计划面上项目(2006B0014Q)

摘  要:针对松香氢化Ni/Al2O3-MxOy催化剂的失活原因,研究了该催化剂的再生方法,得到适宜的工艺条件为:将失活催化剂在550℃焙烧3 h,再用10%硝酸镍溶液浸渍,然后于500℃下焙烧3 h,再于450℃下加氢还原2 h。经再生后的催化剂其催化性能与新鲜催化剂接近。Aiming at the causes for deactivation of Ni/Al2O3-MxOr catalyst used for hydrogenation of gum rosin, the regeneration methods of the catalyst were studied. The appropriate conditions were as follows : the deactivated catalyst was calcined for 3 h at 550 ℃ , followed by impregnation with 10 % nickel nitrate solution, then calcined for 3 h at 500 ℃, and reduced by hydrogenation for 2 h at 450 ℃. The catalytic properties of the regenerated catalyst was close to the fresh catalyst.

关 键 词:松香氢化 Ni/Al2O3-MxOy 催化剂 失活 再生 

分 类 号:TQ351.471[化学工程]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象