金属氢化物-镍电池储存性能衰退的研究  被引量:8

Investigation on degradation of storage characteristics of Ni MH batteries

在线阅读下载全文

作  者:戚道铎[1] 杨勇[1] 林祖赓[1] 

机构地区:[1]厦门大学化学系固体表面物理化学国家重点实验室

出  处:《电源技术》1998年第6期236-239,共4页Chinese Journal of Power Sources

基  金:国家"863"计划资助项目

摘  要:考察了国产金属氢化物-镍电池充放电性能以及电池内阻、隔膜电阻和充电过程中产气量等参数随电池储存时间的变化。通过SEM和XPS分析了电极和隔膜表面形貌及组成的改变,初步讨论了国产电池储存性能下降的原因。结果表明,随着储存期延长,电池放电容量,尤其1.1A电流下放电容量衰退较大,内阻及隔膜电阻增大,充电过程中电池内产气量剧增时间提前,同时正极膨胀变形,隔膜纤维变粗,孔隙减小,且有杂质嵌入,负极表面有氟元素富集。另外。Changes in the charging discharging performance of the Ni MH batteries made in China and related parameters such as internal impedance, gas evolution volume of the battteries during charging process and separator resistance in different periods of storage are investigated in this paper. The surface morphology and composition changes of the electrodes and separators have been analyzed through SEM and XPS technique. The reasons for degradation of storage characteristics of the batteries are discussed. The results show that, with increase in storage period, the discharge capacity, especially when discharging current is 1.1A, degrades seriously, the internal resistance of batteries and separator resistance increase, the gas evolution becomes serious, the positive electrode materials and the separator fiber swell and deform, the holes of separator become smaller with impurities in it and with the increase of the storage period the oxidation on negative electrode is strengthened.

关 键 词:储存性能 衰退 MH-NI电池 碱性蓄电池 

分 类 号:TM912.2[电气工程—电力电子与电力传动]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象