陶瓷涂层断裂韧性的表征  被引量:12

Characterization on Fracture Toughness of Ceramic Coatings

在线阅读下载全文

作  者:武创[1] 郗雨林[1] 王其红[1] 张新杰[1] 

机构地区:[1]中国船舶重工集团公司洛阳船舶材料研究所,河南洛阳471039

出  处:《热加工工艺》2010年第4期109-112,共4页Hot Working Technology

摘  要:由于陶瓷本身的脆性,陶瓷涂层的应用受到了极大的制约。断裂韧性是反映材料抵抗裂纹失稳扩展能力的力学性能指标,陶瓷涂层因为脆性和低维特点,对其断裂韧性的表征存在较大困难,目前主要有临界应力强度因子KⅠC、临界裂纹扩展能量释放率GⅠC和裂纹密度β三种表征方法。本文对上述方法进行了总结、分析。Due to the brittleness of ceramic materials,the application of ceramic coatings is badly influenced.Fracture toughness is a mechanics parameter reflecting material ability of resistance to crack propagation.It is difficult to measure the fracture toughness of ceramic coatings because of their brittleness and 2D characteristics.However,three parameters,critical stress field intensity factor KⅠC,critical strain energy release rate GⅠC and crack density β,can be used to characterize ceramic coating toughness.These methods are described and analyzed.

关 键 词:陶瓷涂层 断裂韧性 表征方法 

分 类 号:TG174.453[金属学及工艺—金属表面处理]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象