镍系SBS加氢反应机理及加氢催化剂制备研究  被引量:4

Study on SBS hydrogenation reaction mechanism with nickel catalyst and the preparation of hydrogenation catalyst

在线阅读下载全文

作  者:贺小进[1] 李伟[1] 梁爱民[1] 陈建军[1] 王爱东[1] 胡保利[1] 石建文[1] 陈淑明[1] 

机构地区:[1]中国石化股份有限公司北京燕山分公司研究院锂系部,北京102500

出  处:《弹性体》2010年第2期32-35,共4页China Elastomerics

基  金:中国石油化工总公司项目(499027)

摘  要:对镍系SBS催化加氢机理进行了探讨,对催化剂制备工艺进行了优化。当催化剂组分质量浓度为2~4 g/L,陈化温度为50~70℃,n(Al)/n(Ni)为3~6时催化剂活性最高。向待加氢胶液中加入一定量破杂剂A可使催化剂活性及稳定性有一定程度提高。用该法制备的催化剂有较好的稳定性,常温下放置一个月其催化活性几乎没有变化。The hydrogenation reaction mechanism of SBS with nickel catalyst was discussed.The preparation of hydrogenation catalyst has been optimized.The catalyst has highest activity when the concentration of catalyst components is the 2~4g/L,aging temperature is 50~70℃,Al/Ni molar ratio is 3~6.The activity and stability of catalyst can be improved when add a certain amount of metallorganic compound A to SBS solution.This catalyst has good stability,its activity did not change when placed one month at room temperature.

关 键 词:加氢催化剂 陈化 活性中心 

分 类 号:TQ334.2[化学工程—橡胶工业]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象