LiCl引入对羟基磷灰石陶瓷耐酸蚀及烧结的影响  被引量:2

Influences of Antacid Capability and Sintering Performance on Hydroxyapatite Ceramic Introduced LiCl

在线阅读下载全文

作  者:卢娟[1] 梁列峰[2] 翁杰[3] 姜法兴[3] 

机构地区:[1]西南大学材料科学与工程学院,重庆400716 [2]西南大学纺织服装学院,重庆400716 [3]西南交通大学材料先进技术教育部重点实验室,成都610031

出  处:《材料导报(纳米与新材料专辑)》2010年第1期395-397,共3页

基  金:重庆市自然科学基金(CSTC-2008BB4096);重庆市教委科学研究计划(KJ060307)

摘  要:在制备羟基磷灰石(HA)陶瓷的初期引入少量LiCl,其乙酸浸蚀失重实验表明,掺杂后HA陶瓷的耐酸蚀能力增强,HA颗粒仍然能保持较强的连接,掺杂后HA陶瓷的显微硬度稳定并有所提高,X射线衍射分析说明引入少量LiCl没有导致HA的分解。A few LiCl is introduced into hydroxyapatite(HA) slurry in initial stages of HA ceramic(HAC) manufacturing. The weight-losing experiment by immersing acetic acid solution indicates that the antacid capability of HAC doped with LiCl increases. The HA grain can connected strongly with each other in the ceramic block. Micro ri gidity of the doped HAC increases and changes steadily in different testing point of the sample. XRD patterns indicates that introducing LiCl doesn't result in decomposing of HA.

关 键 词:LICL 羟基磷灰石陶瓷 耐酸性 烧结性能 

分 类 号:TQ174.75[化学工程—陶瓷工业]

 